Cement pond: glass flake anti-corrosion construction process

Cement pool: Substrate processing → Epoxy coal asphalt heavy anti-corrosion coating (epoxy glass flake heavy anti-corrosion coating) → Inspection and repair defects (including scraper filling) → Epoxy coal asphalt heavy-duty coating (epoxy coal asphalt heavy anti-corrosion coating )→Interlining→Epoxy coal asphalt heavy anti-corrosion coating (or epoxy glass flake heavy anti-corrosion coating)→Interlining→Epoxy coal asphalt heavy anti-corrosion coating (or epoxy glass flake heavy anti-corrosion coating)→Interlining→Epoxy coal asphalt heavy antisepsis Paint (or epoxy glass flake heavy anti-corrosion coating) → Check and repair - epoxy coal asphalt heavy anti-corrosion coating topcoat (or epoxy glass flake heavy anti-corrosion coating) Third, the construction of the sewage pool 1 Sewage tank anti-corrosion sewage pool anti-corrosion cement substrate Treatment: Check the smoothness of the cement surface, remove the old and loose cement layer that is not firmly attached to the pool, and strictly control the curing of the cement on the 28th, the moisture content is less than 8%, use the grinding machine to sharpen the sharp edges, smooth the surface Remove dust completely.

2 brushing closed primer: the use of epoxy coal asphalt special sealing primer, preparation methods: the paint was thoroughly stirred to the bottom of the bucket without sediment, according to the amount of brushing out. If there is a crust, you should first remove the surface crust. Use period: adjusted primer, it is recommended to use within 3 hours. Unfinished primer should not be poured into the original paint.

3 repair using a special putty repair irregularities, so that the overall level to the surface.

4 a paint (ie: an epoxy coal asphalt heavy anti-corrosion coating or epoxy glass flake heavy anti-corrosion coating) Preparation method: the paint is thoroughly stirred to the bottom of the bucket without sediment, press the paint in the stirring state: curing agent is 20:2.5 (Weight ratio), add a special curing agent and mix evenly, and prepare the prepared paint for 10-15 minutes. If the temperature is too low and the viscosity is large, special thinners of 1-5% may be added, and the curing agent may be appropriately increased.

Loose Powder Jar

Loose Powder Jar,Loose Powder Case,Loose Powder Compact Case,Loose Powder Jar With Sifter

SHAOXING CARESO PLASTIC CO., LTD. , https://www.caresoplastic.com